Tungsten, Tantalum & Titanium: High Temp and Corrosion Resistant Alloys
Tungsten, Tantalum & Titanium
High Temperature and Corrosion Resistant Alloys
Tungsten, Tantalum, and Titanium are part of a group of metals known as the refractory metals group. These types of metals are used for their chemical and electrical properties.
TUNGSTEN
Organizations depend on Tungsten and its alloys for their high strength, melting point, and high-density properties, and high temperatures. Tungsten can be used as an additive to enhance physical properties in steel. When used in the aerospace industry, Tungsten and its alloys are applied to blades used on jet engines. In the automotive industry, they are applied to electronics. And, in the military industry, Tungsten is applied to wear-resistant parts. Additional applications extend much farther than these few. In fact, Tungsten weights were used in Mars on a Mars Exploration Rover and Pathfinder.
NOMINAL DATA SHEET
CHEMISTRY
|
PERMISSABLE
VARIONATS IN CHECK ANALYSIS, %
|
MELTING
POINT
|
Tungsten
(W): 99.95%
|
|
3410
C
|
|
|
|
C
- 0.010%
|
+\-
0.002
|
RECRYSTALLATION
|
O
- 0.010%
|
+
10% relative
|
TEMPERATURE
|
N
- 0.010%
|
+0.0005
|
1200
- 1400 C
|
Fe
- 0.010%
|
+0.001
|
|
NI
- 0.010%
|
+0.001
|
|
SI
- 0.010%
|
+0.001
|
|
|
|
|
DENSITY
|
|
|
19.3
gm/cc
|
|
|
[TOP]
TANTALUM
Tantalum is one of the most corrosion resistant metal alloys in the market. Its properties include: tensile strength, yield strength, modulus elasticity, elongation, and Rockwell B Hardness. It can easily be fabricated and is highly conductive of heat and electricity. It’s often used in the automotive industry in electronics and tools such as computers and phones.
NOMINAL DATA SHEET
CHEMICAL
COMPOSITION
|
MECHANICAL
PROPERTIES (MIN)
|
Carbon:
0.010
|
Ultimate
Tensile Strength, min, psi
|
Oxygen:
0.015
|
(Mpa)
|
Nitrogen:
0.010
|
30,000
(207) <0.060 in. thick
|
Hafnium:
0.0015
|
25,000
(172) >0.060 in. thick
|
Niobium:
0.100
|
|
Iron:
0.010
|
Yield
Strength, min, psi, (Mpa)
|
Titanium:
0.010
|
(2%
Offset)
|
Tungsten:
0.05
|
20,000
(138) <0.060 in. thick
|
Molybdenum:
0.020
|
15,000
(103) >0.060 in. thick
|
Silicon:
0.005
|
|
Nickel:
0.010
|
Elongation,
min, %
|
Tantalum:
Remainder
|
(1-in.
Gage Length
|
|
20
<0.060 in. thick
|
|
>0.060
in. thick
|
|
|
|
Density:
16.6 gm/cc
|
[TOP]
TITANIUM
Titanium is extremely durable, corrosion/erosion resistant, and has high intrinsic shock resistance. In addition, it has high fatigue strength when used in the air, is a low-density alloy, and has good thermal conductivity. A variety of industries depend on it including but not limited to: military and defense, aircraft and aerospace, and healthcare. It has been applied to everything from dental implants to consumer electronics.
NOMINAL DATA SHEET
COMMERCIALLY
PURE TITANIUM GRADE #1
|
NOMINAL
DATA SHEET
|
CHEMICAL
COMPOSITION
|
ANNEALED
PROPERTIES (MIN)
|
C
- 0.08
|
Tensile
(psi) - 35,000
|
Fe
- 0.20
|
Yield
(psi) - 25,000
|
N
- 0.03
|
Elongation
%(2") - 24
|
O
- 0.18
|
Reduction
of Area - 30
|
H
- 0.015
|
|
Ti
- Balance
|
HARDNESS
|
Cu
- .50 max
|
RB 70
|
PHYSICAL PROPERTIES(ANNEALED
CONDITION)
Electrical Resistivity at Room Temperature (Microhms
cm) - 56
Modulus of Elasticity - Tension (10(-6) psi)
- 14.9
Melting Point - 3040 F
Density - .163
Modulus of Elasticity - Torsion (10(-6) psi)
- 6.5
Thermal Coductivity (Btu/hr./sq.ft./F/ft.) -
9.0 at Room Temperature
Specific Heat (Btu/lb./F) at Room Temperature
- 0.124
Coefficient of Thermal Expansion, in./in./ F
x 10(-******)
32 - 212
..4.8
32 - 600
..5.1
32 - 1000
5.4
32 - 1200
5.6
32 - 1500
5.6
|
NOMINAL
MECHANICAL PROPERTIES(ANNEALED CONDITION)
|
Bend Radius - 1.5/2.0 x Thickness
Weld Bend Radius - 1.5/2.0 x Thickness
|
COMMERCIALLY
PURE TITANIUM GRADE #2
|
NOMINAL
DATA SHEET
|
CHEMICAL
COMPOSITION
|
ANNEALED
PROPERTIES (MIN)
|
C
- 0.08
|
Tensile
(psi) - 50,000
|
Fe
- 0.25
|
Yield
(psi) - 40,000
|
N
- 0.03
|
Elongation
%(2") - 20
|
O
- 0.20
|
Reduction
of Area - 30
|
H
- 0.015
|
|
Ti
- Balance
|
HARDNESS
|
Cu
- .50 max
|
RB 80
|
PHYSICAL PROPERTIES(ANNEALED
CONDITION)
Electrical Resistivity at Room Temperature (Microhms
cm) - 56
Modulus of Elasticity - Tension (10(-6) psi)
- 14.9
Melting Point - 3020 F
Density - .163
Modulus of Elasticity - Torsion (10(-6) psi)
- 6.5
Thermal Coductivity (Btu/hr./sq.ft./F/ft.) -
9.0 at Room Temperature
Specific Heat (Btu/lb./F) at Room Temperature
- 0.124
Coefficient of Thermal Expansion, in./in./ F
x 10(-******)
32 - 212
..4.8
32 - 600
..5.1
32 - 1000
5.4
32 - 1200
5.6
32 - 1500
5.6
|
NOMINAL
MECHANICAL PROPERTIES(ANNEALED CONDITION)
|
Bend Radius - 2.0/2.5 x Thickness
Weld Bend Radius - 2.0/3.0 x Thickness
|
COMMERCIALLY
PURE TITANIUM GRADE #4
|
NOMINAL
DATA SHEET
|
CHEMICAL
COMPOSITION
|
ANNEALED
PROPERTIES (MIN)
|
C
- 0.08
|
Tensile
(psi) - 50,000
|
Fe
- 0.50
|
Yield
(psi) - 70,000
|
N
- 0.05
|
Elongation
%(2") - 15
|
O
- 0.40
|
Reduction
of Area - 25
|
H
- 0.015
|
|
Ti
- Balance
|
HARDNESS
|
|
RB 80
|
PHYSICAL PROPERTIES(ANNEALED
CONDITION)
Electrical Resistivity at Room Temperature (Microhms
cm) - 60
Modulus of Elasticity - Tension (10(-6) psi)
- 15.1
Melting Point - 3020 F
Density - .163
Modulus of Elasticity - Torsion (10(-6) psi)
- 6.5
Thermal Coductivity (Btu/hr./sq.ft./F/ft.) -
9.0 at Room Temperature
Specific Heat (Btu/lb./F) at Room Temperature
- 0.129
Coefficient of Thermal Expansion, in./in./ F
x 10(-******)
32 - 212
..4.8
32 - 600
..5.1
32 - 1000
5.4
32 - 1200
5.6
32 - 1500
5.6
|
NOMINAL
MECHANICAL PROPERTIES(ANNEALED CONDITION)
|
Bend Radius - 2.5/3.0 x Thickness
Weld Bend Radius - 3.0/5.0 x Thickness
|
TITANIUM
GRADE 6AL/4V
|
NOMINAL
DATA SHEET
|
CHEMICAL
COMPOSITION
|
ANNEALED
PROPERTIES (MIN)
|
C
- 0.08
|
Tensile
(psi) - 130,000
|
Fe
- 0.25
|
Yield
(psi) - 120,000
|
N
- 0.05
|
Elongation
%(2") - 10
|
O
- 0.20
|
Reduction
of Area - 25
|
H
- 0.015
|
|
Ti
- Balance
|
HARDNESS
|
AL
- 5.50/6.75
|
RB
36
|
V
- 3.5/4.5
|
|
PHYSICAL PROPERTIES(ANNEALED
CONDITION)
Electrical Resistivity at Room Temperature (Microhms
cm) - 60
Modulus of Elasticity - Tension (10(-6) psi)
- 15.1
Melting Point - 3020 F
Density - .163
Modulus of Elasticity - Torsion (10(-6) psi)
- 6.5
Thermal Coductivity (Btu/hr./sq.ft./F/ft.) -
9.0 at Room Temperature
Specific Heat (Btu/lb./F) at Room Temperature
- 0.129
Coefficient of Thermal Expansion, (10(-6) in/in/F)
32 - 212
..5.0
32 - 600
..5.3
32 - 1000
5.6
32 - 1200
5.9
32 - 1500
6.1
|
NOMINAL
MECHANICAL PROPERTIES(ANNEALED CONDITION)
|
Bend Radius - 4.5/5.0 x Thickness
Weld Bend Radius - 6.0/10.0 x Thickness
|
AVAILABLE
GRADES
|
CP
GRADES 1-4, 6AL4V, 3AL2.5V, ELI
|
[TOP]
|